# 1MW test measurement ###### tags: `Experiment` `1MW` `Log` `Instrumental` ## measurement(2020/06/26) ### conditions Sample : Ba(Fe,Sc)$_{12}$O$_{19}$, x=0.033 Size : 2.0 $\times$ 2.0 $\times$ 1mm$^{3}$ Acc. Power : 910kW Frame : 1.5th   T : sweap down to the bottom temperature@0.5K/min. meas. : 60 sec./run Run# : 17798-18340 *17798-18040 in Det#17 *18113-18192 in Det#20 *18194-18340 in Det#17 ### Laue pattern(Run#17798)  c* is in Det#17 ### Results #### profile(along c*-axis)  Brow-up ((0 0 8.7) and (0 0 9.3))  #### Temperature dependence of magnetic reflection  #### Temperature and omega angles  #### Omega trace  #### Hovering reflection Run#17798(det#17)  Run#17900(det#17)  Run#18000(det#17)  Run#18130(det#20)  Run#18192(det#20) 
×